Guide
What is the yield strength of steel, and which value belongs on your drawing?
The yield strength of steel is the stress at which it stops springing back and starts to deform permanently, defined for most steels at 0.2 percent plastic strain. Short answer: the number that belongs in design and on the drawing is the specification minimum for the grade, product form and condition you order, not a typical datasheet value; a cold-drawn 1018 bar, for example, is typically quoted at 54,000 psi yield at 1 in diameter, but that is an estimate that varies with bar size and drawing practice, while a heat-treated alloy steel's minimum depends on the strength level it is treated to.
By Saola Manufacturing engineering team · Published · Updated
Grade comparisons are covered elsewhere: 1018 vs 1045 and 4140 vs 4340. Reading the certificate that proves the value is covered in how to read a mill test report. This page explains what yield strength is, which numbers are minimums and which are not, and how to specify and check it.
On this page
What is yield strength, and how is it different from tensile strength?
Yield strength marks the start of permanent deformation; tensile (ultimate) strength is the highest stress the steel carries before it necks and breaks. Parts are sized so working stress stays well below yield.
MIL-HDBK-5J explains that some ferrous alloys show a sharp yield point, where the material stretches with no rise in stress, while most high-strength steels yield gradually; for those, industry adopted a plastic strain of 0.002 in/in as the limit, and the yield stress is read where a line parallel to the elastic part of the curve, offset by that strain, meets the stress-strain curve (MIL-HDBK-5J, Section 1.4.4.3). That is the familiar “0.2 percent offset yield”.
The gap between yield and tensile strength matters for the part. The table below shows the gap: in high-strength heat-treated steels the minimum yield sits close to the tensile strength, while annealed or cold-drawn steels show a wider margin between the two. For bolted joints, press fits and parts that must not take a permanent set, yield is the governing number. Tensile testing itself is done to ASTM A370, the test methods and definitions for mechanical testing of steel products (ASTM A370-24).
What yield strength do common steel grades have?
It depends on the condition more than the grade name: per MIL-HDBK-5J the same 4130 runs from 70 to 75 ksi minimum yield normalized and tempered, depending on thickness, to 165 ksi quenched and tempered. Always read the value for the condition you buy.
The table lists specification minimums (S-basis) from MIL-HDBK-5J for alloy and precipitation-hardening steels, plus one typical value for cold-drawn 1018 from the Precision Machined Products Association, which cites SAE J1397 estimated properties (PMPA, 2011). Note the different bases: the 1018 figure is not a minimum. The handbook also says its heat-treated alloy steel values apply only to parts whose tensile strength has been substantiated by adequate quality control testing.
| Steel, form and condition | Basis | Fty, ksi | Ftu, ksi |
|---|---|---|---|
| 1018, cold drawn bar, 1 in diameter | typical (estimate) | 54 | 64 |
| AISI 4130 sheet, strip, plate and tubing, normalized and tempered, up to 0.188 in | minimum (S) | 75 | 95 |
| AISI 4130 tubing, quenched and tempered to 125 ksi, wall up to 0.188 in | minimum (S) | 100 | 125 |
| AISI 4130 tubing, quenched and tempered to 180 ksi, all walls | minimum (S) | 165 | 180 |
| AISI 4340, vacuum-melted (AMS 6414), bar, forging, tubing, quenched and tempered to 260 ksi, section limits apply | minimum (S) | 217 | 260 |
| 17-4PH sheet, strip and plate, H1150 (LT) | minimum (S) | 105 | 135 |
| 17-4PH sheet, strip and plate, H900 (LT) | minimum (S) | 170 | 190 |
| AISI 301 stainless sheet, annealed (L) | minimum (S) | 26 | 73 |
Why do typical values and specification minimums differ so much?
A typical value describes an average bar; a minimum is what every accepted lot must meet. For cold-finished carbon steel the spread is wide because the amount of cold work changes with size and drawing practice.
The PMPA article points out that the SAE J1397 figures are estimated values, not minimums, and gives three reasons properties vary between shipments of the same grade and size: the melting route and residual elements, the amount of cold work (smaller bars at a standard draft get more of it, and suppliers use different drafts), and straightening, which can relax the bar. It reports 1018 seen with yield strength in the high 70,000s psi at 3/8 in diameter and about 42,000 psi at 4 in diameter (PMPA).
The practical rule: if your calculation needs a yield value, take it from the specification and condition you will order, and if that specification has no guaranteed tensile properties for your form, put a minimum on the purchase order and ask for test results. Do not size a part on a datasheet's typical number and then accept material on a certificate that only shows chemistry.
What about 1045, 12L14, 4140, 304 and 316?
Their yield strength is set by the product specification and condition you order: hot-rolled, cold-drawn, annealed, or quenched and tempered. There is no single number per grade, so this page does not give one.
Carbon and alloy bar such as 1045, 12L14 and 4140 can be bought cold-finished to ASTM A108, the specification for cold-finished carbon and alloy steel bar (ASTM A108-24), or hot-rolled and then heat treated. Stainless bars such as 304 and 316 are commonly bought to ASTM A276, the specification for stainless steel bars and shapes, where the mechanical requirements depend on the condition ordered (ASTM A276/A276M-25). Read the minimum from the edition and condition you call out, or from the test results on the supplier's certificate.
Free-machining grades such as 12L14 are usually specified for machinability (see 12L14 vs 1215); if a 12L14 part is loaded, check the yield you can actually guarantee for that bar size. For heat-treated 4140, the strength level is chosen by tempering, so the drawing should state either a hardness range or a minimum strength and how it is verified.
How do you specify yield strength on a drawing or purchase order?
Call the grade, the material specification and the condition. Add a minimum yield only when you need more than the specification guarantees, and then say how it is tested.
- Material: grade plus specification and condition, for example a cold-finished bar to ASTM A108 or a stainless bar to ASTM A276 in the annealed condition.
- If strength matters and the specification does not guarantee it: “minimum yield strength (0.2 percent offset) and minimum tensile strength per ASTM A370, test results on the certificate”, with the values from your analysis.
- For heat-treated parts: a hardness range on the finished part, and, if strength is critical, tensile tests on a coupon from the same heat and heat-treat lot.
- Size class: if your stress analysis assumed a particular bar size, say so, because properties of cold-finished bar change with size.
Avoid copying a datasheet typical value onto the drawing as a minimum. Some lots will be below it, and the result is either rejected material or a quiet waiver.
How do you verify yield strength on steel you receive?
Check the mill test report: heat number, specification and condition, and tested yield and tensile values against the minimum you ordered. On finished parts, a hardness test is a common indirect check.
A certificate that lists chemistry only does not prove strength. Look for the tension test results, the test direction and location if the specification defines them, and a heat number that matches the bar tags. For machined parts, a tensile specimen can rarely be cut from the part itself, so a witness coupon or extra length from the same heat is the way to test after heat treatment. A hardness reading on the part is a common way to confirm that the heat treatment happened, and the mill test report guide covers what each field means.
Which steels can Saola turn, and how is strength documented?
The bar list for CNC turning at our lead plant includes 12L14, C1117 and 52100 steel; other grades and conditions are confirmed at drawing review. Material certification is available on request.
Small turned bar parts run at the lead CNC plant in Vietnam, described on the CNC turning page, which also lists DOM steel tube; milled parts are on the CNC milling page. If your drawing calls a grade or condition that is not on that list, such as 4140 or 316, we confirm the material at drawing review rather than assume it. If you need tested yield and tensile values on the certificate, say so in the quote request. First-article inspection reports for new parts and a dimensional inspection record per lot are available on request.
Frequently asked
Is yield strength the same as yield point?
Not exactly. A yield point is the sharp break some low-carbon steels show; yield strength by the 0.2 percent offset method is used when the curve bends gradually. MIL-HDBK-5J describes both.
How do I convert ksi to MPa?
Multiply by about 6.895. Use the metric value from a metric specification where one exists, rather than converting a typical value.
Does heat treatment change the yield strength?
Yes, a great deal for hardenable steels: the handbook minimums for 4130 and 17-4PH above change with condition. Stiffness does not change, which is a separate question.
Why is my certificate value much higher than the datasheet?
Small cold-drawn bars often test well above the typical value because of the extra cold work. It is real for that lot, but do not design on it for the next one.
Sources
- MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures, U.S. Department of Defense, 2003 (Section 1.4.4.3; Tables 2.3.1.0(c1), (c2), (f1), 2.6.9.0(b), 2.7.1.0(b))
- Three Reasons Why Mechanical Properties of Cold-Drawn Steel Can Vary, Miles Free, Precision Machined Products Association, Production Machining, May 2011
- ASTM A370-24, Test Methods and Definitions for Mechanical Testing of Steel Products, ASTM International, 2024
- ASTM A108-24, Steel Bar, Carbon and Alloy, Cold-Finished, ASTM International, 2024
- ASTM A276/A276M-25, Stainless Steel Bars and Shapes, ASTM International, 2025