RoHS material control Vietnam country-of-origin documentation rfq@saolamfg.comEmail WhatsApp +84 86 501 7914

Guide

What is the 6061-T6 yield strength, and which value should you design and inspect to?

Short answer

6061-T6 yield strength is the stress at which solution heat-treated and artificially aged 6061 aluminum starts to deform permanently, and for design it is quoted as a guaranteed minimum that depends on the product form and thickness. Short answer: for rolled or drawn bar and rod, drawn tube and plate up to 2 in thick, the specification minimum tensile yield in MIL-HDBK-5J is 35 ksi, with an ultimate of 42 ksi; datasheets quoting a higher number are usually giving typical values, which are fine for estimates but not for design margins or incoming inspection.

By Saola Manufacturing engineering team · Published · Updated

The T6 versus T651 temper question is covered in 6061-T6 vs T651, and how to check temper on a finished part in verifying aluminum temper. This page is the numbers page: which strength to use, where it comes from, and what changes it.

On this page

What yield strength does 6061-T6 have by product form?

The design minimum is about the same across bar, tube and thinner plate, while die forgings have a lower ultimate. The table gives the MIL-HDBK-5J values engineers most often need.

MIL-HDBK-5J lists design mechanical properties for 6061 by product form, specification and thickness, with the minimum tensile ultimate (Ftu), tensile yield (Fty) and elongation, plus modulus and density (MIL-HDBK-5J, Tables 3.6.2.0(b2), (c1), (d) and (e)). It also warns that for extrusions the properties should be based on the thickness at the time of quenching, before machining, because selecting values by final machined thickness may be unconservative. The same logic applies when a thin part is machined out of thick stock: the stock's thickness class is what governs.

What are the other key 6061-T6 properties for design?

Modulus of about 9.9 x 10³ ksi in tension, Poisson's ratio 0.33 and density 0.098 lb/in³ per MIL-HDBK-5J, regardless of product form. Stiffness does not change with temper, so moving from T6 to a stronger alloy does not make a part stiffer.

The table combines the strength minimums and the physical constants from the handbook. “S” means the specification minimum; “A” and “B” are statistically based values, explained in the next section.

6061 minimum design properties, longitudinal unless noted, per MIL-HDBK-5J (2003), Tables 3.6.2.0(b2), (c1), (d), (e)
Product form and temperThicknessBasisFtu, ksiFty, ksiElongation (L), %
Rolled, drawn or cold-finished bar and rod, T6 / T651up to 8.000 inS423510
Drawn tube, T6wall 0.025–0.500 inS4235see handbook
Plate, T651 (strength in LT direction)0.250–2.000 inA / B42 / 4335 / 37see handbook
Plate, T651 (strength in LT direction)4.001–6.000 inS40356
Die forging, T6 / T652up to 4.000 inS38357
All forms above: E / Ec / GModulus, 10³ ksi9.910.13.8
All forms above: density, Poisson's ratiolb/in³; μ0.0980.33

What is the difference between minimum, A-basis, B-basis and typical values?

S-basis is the specification minimum, A-basis and B-basis are statistical floors from test data, and typical values are averages. Design and acceptance should use a minimum; typical numbers belong in rough estimates only.

MIL-HDBK-5J defines S-basis as the specification minimum of the governing industry or government specification; B-basis as a value that at least 90 percent of the population is expected to equal or exceed with 95 percent confidence; and A-basis as the lower of the statistical value that at least 99 percent of the population equals or exceeds (with 95 percent confidence) and the specification minimum (MIL-HDBK-5J, Section 9 definitions). Typical values in supplier datasheets are not on that list: they describe an average lot, so roughly half of real material is below them.

The practical consequences are simple. A mill certificate is checked against the minimum in the ordered specification, not against a datasheet. A safety factor applied to a typical value is smaller than it looks. And if a supplier's datasheet quotes a yield well above 35 ksi for 6061-T6, ask whether it is a typical value before putting it in a calculation. Note also that MIL-HDBK-5J was replaced by the MMPDS handbook series, so new aerospace work should use the current MMPDS edition.

What happens to 6061-T6 yield strength after welding?

It drops in the heat-affected zone, because welding heat over-ages or anneals the T6 condition next to the bead. The handbook values above do not apply to a welded joint.

MIL-HDBK-5J notes that when heat-treated or work-hardened aluminum is welded, a loss of mechanical properties generally occurs, and that the extent of the loss (if the part is not re-heat-treated) has to be established for each specific situation (MIL-HDBK-5J, Section 3.1.3.4). In practice, structural welding codes publish reduced as-welded strengths for heat-treatable alloys, and designers use those for the joint area while using the T6 values away from it.

For a machined weldment, three choices follow. Design the welded region to the reduced as-welded strength from the governing welding code. Move welds to low-stress areas. Or solution heat treat and age the whole weldment after welding, which restores much of the strength but can distort the part, so it must happen before final machining. Filler alloy choice also matters for both strength and the appearance of any later anodize.

How should the drawing call out 6061-T6 and its strength?

Call the alloy, temper and material specification for the product form, for example “6061-T6511 per ASTM B221” or “6061-T651 per ASTM B209”, and ask for a mill certificate. Do not write a yield value on the drawing unless it is a real extra requirement.

The material specification already carries the minimum properties for each form and thickness: ASTM B209 for sheet and plate, ASTM B211 for rolled or cold-finished bar, rod and wire, and ASTM B221 for extruded bar, rod, shapes and tube (ASTM B221-21; ASTM B209/B209M-21a; ASTM B211/B211M-19). A yield number on the drawing that copies a datasheet value either repeats the specification or, worse, asks for a typical value as a minimum, which some lots will fail.

If the part is sized close to the limit, say which direction and which thickness class the stress analysis used, so the material can be bought and tested accordingly. The Aluminum Association publishes the alloy and temper registrations behind all of these documents (Aluminum Association standards).

How do you verify 6061-T6 strength on parts you receive?

Check the mill certificate against the ordered specification, and on finished parts check hardness and electrical conductivity to confirm the temper. A tensile test needs a specimen, which a finished part rarely has.

The certificate should show the alloy, temper, specification, heat or lot number and tested tensile results for that lot. On a machined part you cannot pull a tensile bar, so temper is checked indirectly: hardness plus conductivity together tell a T6 part from an annealed or T4 part, as the temper verification guide explains. If the drawing requires proof of strength on the finished part itself, plan for extra material or a witness coupon cut from the same bar and heat lot.

Remember what can change the temper after the mill: welding, as above, and any process that heats the part, such as some coating cure cycles or hot forming. Ask the supplier to declare any heating operation in the route.

Can Saola machine 6061-T6 parts?

Yes: 6061-T6 is on the bar list for CNC turning at our lead plant in Vietnam, and material certification is available on request.

The CNC turning page lists 6061-T6 and 2011-T3 among the bar materials run at the lead CNC plant for small bar parts; milled 6061 parts are reviewed case by case against the CNC milling page. First-article inspection reports for new parts and a dimensional inspection record per lot are available on request, and the mill certificate for the bar can be supplied on request. If your design depends on a particular product form or thickness class, put it on the drawing and we will confirm the stock at drawing review. Send the drawing through the quote form.

Frequently asked

What is 6061-T6 yield strength in MPa?

The 35 ksi minimum per MIL-HDBK-5J converts to about 241 MPa (1 ksi = 6.895 MPa). Use the metric value from the metric specification you order to, rather than converting a typical value.

Is 6061-T651 stronger than 6061-T6?

No. MIL-HDBK-5J lists the same bar minimums for T6 and T651; the difference is stress relief by stretching, which reduces distortion during machining.

Does 6061-T6 get weaker at high temperature?

Yes. MIL-HDBK-5J gives curves for the effect of temperature on 6061-T6 strength; check them if the part runs hot, and remember that long exposure can also over-age the temper.

Why is the forging ultimate strength lower?

Each product form has its own specification and test basis. Use the value for the form you actually buy, not the highest number you can find.

Sources

  1. MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures, U.S. Department of Defense, 2003 (Section 3.1.3.4, Section 3.6.2, Section 9 definitions)
  2. ASTM B221-21, Aluminum and Aluminum-Alloy Extruded Bars, Rods, Wire, Profiles, and Tubes, ASTM International, 2021
  3. ASTM B209/B209M-21a, Aluminum and Aluminum-Alloy Sheet and Plate, ASTM International, 2021
  4. ASTM B211/B211M-19, Aluminum and Aluminum-Alloy Rolled or Cold-Finished Bar, Rod, and Wire, ASTM International, 2019
  5. Standards, The Aluminum Association, accessed 2026

Have a drawing for this? Send it for a quote.

STEP or PDF, one part or a whole family. You get a unit price at your volume, the tooling cost, and a short manufacturability note.