RoHS material control Vietnam country-of-origin documentation rfq@saolamfg.comEmail WhatsApp +84 86 501 7914

Guide

What is the difference between 410, 420 and 440C stainless steel for a machined part?

Short answer

410, 420 and 440C stainless steel are martensitic stainless grades: chromium steels with enough carbon to be hardened by quenching and tempering, unlike 304 or 316. Short answer: carbon rises from 410 to 420 to 440C, and with it the hardness and wear resistance after heat treatment, while toughness and machinability fall; all three resist corrosion less than 316, so pick the lowest-carbon grade that meets the hardness or wear requirement.

By Saola Manufacturing engineering team · Published · Updated

Free-machining 416 is covered in a separate guide, and the ferritic alternative in 304 vs 430 stainless. This page compares the three standard hardenable grades and how to specify them.

On this page

What makes 410, 420 and 440C different from 304 and 316?

They harden by heat treatment the way carbon and alloy steels do, because they contain deliberate carbon and no large nickel addition. That gives strength and wear resistance but costs corrosion resistance and weldability.

The British Stainless Steel Association describes martensitic stainless steels as similar to low-alloy or carbon steels: carbon is added on purpose so they can be hardened and strengthened by heat treatment, they are ferromagnetic, the main alloying element is chromium, and the strength reached by heat treatment depends on the carbon content, with higher-carbon grades able to reach around 60 HRC (BSSA, Martensitic stainless steels). In the annealed condition they are relatively soft, and the same source notes they are usually machined, cold formed or cold worked in that condition.

Corrosion is the trade-off. BSSA states that martensitic grades generally resist corrosion less than other stainless types, that higher-chromium martensitic grades such as 431 come close to 304 in many environments, and that no martensitic stainless steel compares with 316 (BSSA, Martensitic Stainless Steels, 2021). The BSSA article also notes that optimum corrosion resistance is reached in the hardened and tempered condition (BSSA, Martensitic stainless steels).

How do 410, 420 and 440C compare in composition and strength?

410 is the low-carbon grade, 420 covers a range of carbon levels with strength rising as carbon rises, and 440C has about 1 percent carbon against about 0.1 percent for 410, plus more chromium. The European long-product standard specifies minimum quenched and tempered properties for 410 and 420 but none for 440C.

The table reproduces the EN 10088-3 values summarized by BSSA, with the nearest AISI names it gives. PS is the minimum proof (yield) strength at the standard plastic-strain offset. For 440C (1.4125) the standard defines no quenched and tempered properties, which BSSA notes is common for the very high carbon grades, so hardness for 440C has to come from the supplier or the heat treat specification.

Martensitic stainless long products, quenched and tempered (QT), up to 160 mm diameter · values per EN 10088-3 as summarized by the British Stainless Steel Association (2021)
EN number (AISI)C, %Cr, %Condition0.2% PS min, MPaTensile, MPaElongation min, %
1.4006 (410)0.08–0.1511.5–13.5QT650450650–85012
1.4021 (420)0.16–0.2512.0–14.0QT700500700–85013
1.4028 (420)0.26–0.3512.0–14.0QT850650850–100010
1.4031 (420)0.36–0.4212.5–14.5QT800650800–100010
1.4125 (440C)0.95–1.2016.0–18.0No QT properties defined in the standard; Mo 0.40–0.80

Which grade fits which part?

Use 410 for moderate strength with the highest toughness of the three, 420 when you need a harder surface or edge, and 440C for maximum hardness and wear, such as bearing and cutting-edge duty. Move up in carbon only when the duty demands it.

BSSA lists blades and cutting tools, surgical instruments, gears, valves, pumps, shafts and bearings among martensitic applications, and points out the 12 percent chromium series in which rising carbon from 1.4021 to 1.4034 brings higher strength with a loss of impact toughness (BSSA, 2021). In practice the choice comes down to three questions:

  • What hardness does the function need? Wear surfaces and edges push toward 420 or 440C; a shaft or pin that mainly needs strength may be fine in 410.
  • How corrosive is the service? If the environment needs 304 or 316, a martensitic grade is the wrong family, whatever its hardness; consider a precipitation-hardening grade or a different design.
  • Will the part be welded or impact-loaded? Higher carbon means poorer weldability and lower toughness, which BSSA notes requires pre and post heat treatment in welding.

How machinable are 410, 420 and 440C?

Annealed 410 machines about as well as 304, and 440C has the lowest machinability index in BSSA's comparison. If machinability drives cost and the hardness need is modest, 416 is the free-machining alternative.

BSSA's machinability index for annealed stainless steels, relative to a free-machining low-alloy steel at 1.0, gives 0.50 for 410, 0.40 for 440C, 0.52 for 304 and 0.95 for free-machining 416 (BSSA, Influence of steel family on machinability). The same article notes the indices only rank steel types, because achievable speeds and feeds also depend on the method, tool and lubrication.

Sequence matters as much as grade. BSSA notes these grades are usually machined in the annealed condition and hardened afterwards. Where hardening distortion would affect tight features, call for grinding or finish machining after heat treatment and leave stock for it. Put that sequence on the drawing or let the supplier propose it at drawing review, and say which features must hold size after hardening.

How should the drawing call out a martensitic stainless part?

Name the grade and bar specification, the heat treated condition as a hardness range on the finished part, and any passivation. A grade name alone leaves the most important property, hardness, undefined.

  • Material: grade with UNS number and the bar specification, for example ASTM A276 for stainless bars and shapes, or ASTM A582 for free-machining stainless bars such as 416 (ASTM A276/A276M-25; ASTM A582/A582M-22).
  • Heat treatment: “harden and temper to” a hardness range, where it is measured, and whether a tensile coupon is required. For 440C give the hardness explicitly, since the European bar standard defines no hardened properties for it.
  • Finish sequence: which features are ground or machined after hardening.
  • Passivation, if required, to ASTM A967, with the method left to the processor or stated, and any salt-spray or humidity acceptance test (ASTM A967/A967M-25).

On receipt, check the material certificate against the grade, then hardness on the part at the stated location. A magnet does not tell 410 from 420 or 440C, because all martensitic grades are ferromagnetic.

Can Saola machine 410, 420 or 440C parts?

These grades are not on the turning page's bar list, so the grade, its condition and the hardening route are confirmed at drawing review for each part. Passivation is not on our current finish menu either.

Turned parts run on conventional CNC lathes at our lead CNC plant in Vietnam, as described on the CNC turning page, and milled parts on the CNC milling page. Because 410, 420 and 440C are not on the listed bar materials, we confirm availability and the route for hardening and any finishing at drawing review rather than assume them. First-article inspection reports for new parts, a dimensional inspection record per lot and material certification are available on request. Send the drawing with the hardness requirement through the quote form.

Frequently asked

Is 420 stainless magnetic?

Yes. BSSA classes martensitic stainless steels as a hard ferromagnetic group, so 410, 420 and 440C are all attracted to a magnet.

Why does the 420 grade appear several times in the table?

The European standard splits AISI 420 into several numbered grades by carbon range, from 1.4021 to 1.4034. If you order “420”, state the carbon range or EN number you expect, because hardness potential follows carbon.

Is 440C more corrosion resistant than 410?

It has more chromium on paper, but BSSA places martensitic grades as a family below the other stainless types for corrosion, and states that none compares with 316. Treat both as moderate-corrosion grades and test in your environment if it matters.

Can martensitic stainless be used in the annealed condition?

It can, but you then pay for a hardenable grade without using its strength, and BSSA notes optimum corrosion resistance is reached after hardening and tempering. If no hardness is needed, a ferritic or austenitic grade is usually the better choice.

Sources

  1. Martensitic Stainless Steels (EN 10088-3 grade summary), British Stainless Steel Association, 2021
  2. Martensitic Stainless Steels, British Stainless Steel Association, accessed 2026
  3. Influence of steel family (type) on machinability, British Stainless Steel Association, accessed 2026
  4. ASTM A276/A276M-25, Stainless Steel Bars and Shapes, ASTM International, 2025
  5. ASTM A582/A582M-22, Free-Machining Stainless Steel Bars, ASTM International, 2022
  6. ASTM A967/A967M-25, Chemical Passivation Treatments for Stainless Steel Parts, ASTM International, 2025

Have a drawing for this? Send it for a quote.

STEP or PDF, one part or a whole family. You get a unit price at your volume, the tooling cost, and a short manufacturability note.